Absaye kayan fari
- Launi:Fari mai tsafta
- Siffar:Cubic da Angular da Sharp
- Takamaiman Nauyi:3.95
- Mohs Hardness:9.2 Mohs
- Wurin narkewa:2150 ℃
- Yawan yawa:1.50-1.95g/cm3
- Al2O3:99.4% Min
- Na 2O:0.30% Max
-
Wfa White Fused Alumina/Aluminum Oxide/Alumina Oxide/Corundum
- ALO3:99.5%
- TiO2:0.0995%
- SiO2 (ba kyauta):0.05%
- Fe2:0.08%
- MgO:0.02%
- Alkali (Soda & Potash):0.30%
- Fom Crystal:Matsayin Rhombohedral
- Yanayin Sinadari:Amphoteric
- Takamaiman Nauyi:3.95 gm/c
- Yawan Yawa:116 lbs/ft3
- Tauri:KNOPPS = 2000, MOHS = 9
- Wurin narkewa:2,000°C
-
Daidaitaccen simintin simintin gyare-gyare na ƙwanƙwasa ƙwanƙwasa Farin Corundum 280 Mesh 320 Mesh
- ALO3:99.5%
- TiO2:0.0995%
- SiO2 (ba kyauta):0.05%
- Fe2:0.08%
- MgO:0.02%
- Alkali (Soda & Potash):0.30%
- Fom Crystal:Matsayin Rhombohedral
- Yanayin Sinadari:Amphoteric
- Takamaiman Nauyi:3.95 gm/c
- Yawan Yawa:116 lbs/ft3
- Tauri:KNOPPS = 2000, MOHS = 9
- Wurin narkewa:2,000°C
-
JIS Daidaitaccen Farin Fused Alumina don Rufin Cloth Abrasives Farin Fused Alumina Wfa
- ALO3:99.5%
- TiO2:0.0995%
- SiO2 (ba kyauta):0.05%
- Fe2:0.08%
- MgO:0.02%
- Alkali (Soda & Potash):0.30%
- Fom Crystal:Matsayin Rhombohedral
- Yanayin Sinadari:Amphoteric
- Takamaiman Nauyi:3.95 gm/c
- Yawan Yawa:116 lbs/ft3
- Tauri:KNOPPS = 2000, MOHS = 9
- Wurin narkewa:2,000°C
-
Farin Corundum JIS/White Fused Alumina/Wa Abrasive
- ALO3:99.5%
- TiO2:0.0995%
- SiO2 (ba kyauta):0.05%
- Fe2:0.08%
- MgO:0.02%
- Alkali (Soda & Potash):0.30%
- Fom Crystal:Matsayin Rhombohedral
- Yanayin Sinadari:Amphoteric
- Takamaiman Nauyi:3.95 gm/c
- Yawan Yawa:116 lbs/ft3
- Tauri:KNOPPS = 2000, MOHS = 9
- Wurin narkewa:2,000°C
-
Maɗaukakin Maɗaukaki Mai Inganci Farin Fused Alumina Grits tare da Samfurin Kyauta
- ALO3:99.5%
- TiO2:0.0995%
- SiO2 (ba kyauta):0.05%
- Fe2:0.08%
- MgO:0.02%
- Alkali (Soda & Potash):0.30%
- Fom Crystal:Matsayin Rhombohedral
- Yanayin Sinadari:Amphoteric
- Takamaiman Nauyi:3.95 gm/c
- Yawan Yawa:116 lbs/ft3
- Tauri:KNOPPS = 2000, MOHS = 9
- Wurin narkewa:2,000°C