Zirconia foda yana da halaye na high taurin, high-zazzabi juriya, sinadaran lalata juriya, sa juriya, kananan thermal conductivity, karfi thermal girgiza juriya, mai kyau sinadaran kwanciyar hankali, fice m abu, da dai sauransu The Properties na kayan za a iya inganta ta hada nanometer zirconia tare da alumina da silicon oxide. Nano zirconia ba wai kawai ana amfani dashi a cikin tukwane na tsari da yumbu na aiki ba. Nano zirconia doped da abubuwa daban-daban conductive kaddarorin, amfani da m baturi lantarki masana'antu.
Kaddarorin jiki
Matsayin narkewa sosai
Tsabar sinadarai a yanayin zafi mai girma
Low thermal fadada idan aka kwatanta da karafa
Babban juriya na inji
Juriya abrasion
Juriya na lalata
Oxide ion conductivity (lokacin da aka tabbatar)
Chemical inertia
| Nau'in Kayayyakin | Nau'in samfur | ||||
| Haɗin Sinadari | ZrO2 na al'ada | Babban tsarki ZrO2 | 3Y ZrO2 | 5Y ZrO2 | 8Y ZrO2 |
| ZrO2+HfO2 % | ≥99.5 | ≥99.9 | ≥94.0 | ≥90.6 | ≥86.0 |
| Y2O3 % | --- | --- | 5.25± 0.25 | 8.8± 0.25 | 13.5 ± 0.25 |
| Al2O3 % | <0.01 | <0.005 | 0.25± 0.02 | <0.01 | <0.01 |
| Fe2O3% | <0.01 | <0.003 | <0.005 | <0.005 | <0.01 |
| SiO2 % | <0.03 | <0.005 | <0.02 | <0.02 | <0.02 |
| TiO2% | <0.01 | <0.003 | <0.005 | <0.005 | <0.005 |
| Haɗin Ruwa (wt%) | <0.5 | <0.5 | <1.0 | <1.0 | <1.0 |
| LOI(wt%) | <1.0 | <1.0 | <3.0 | <3.0 | <3.0 |
| D50(μm) | <5.0 | <0.5-5 | <3.0 | <1.0-5.0 | <1.0 |
| Yankin saman (m2/g) | <7 | 3-80 | 6-25 | 8-30 | 8-30 |
| Nau'in Kayayyakin | Nau'in samfur | ||||
| Haɗin Sinadari | 12Y ZrO2 | Yau YdaidaitaZrO2 | Bakar YdaidaitaZrO2 | Nano ZrO2 | Thermal fesa ZrO2 |
| ZrO2+HfO2 % | ≥79.5 | ≥94.0 | ≥94.0 | ≥94.2 | ≥90.6 |
| Y2O3 % | 20± 0.25 | 5.25± 0.25 | 5.25± 0.25 | 5.25± 0.25 | 8.8± 0.25 |
| Al2O3 % | <0.01 | 0.25± 0.02 | 0.25± 0.02 | <0.01 | <0.01 |
| Fe2O3% | <0.005 | <0.005 | <0.005 | <0.005 | <0.005 |
| SiO2 % | <0.02 | <0.02 | <0.02 | <0.02 | <0.02 |
| TiO2% | <0.005 | <0.005 | <0.005 | <0.005 | <0.005 |
| Haɗin Ruwa (wt%) | <1.0 | <1.0 | <1.0 | <1.0 | <1.0 |
| LOI(wt%) | <3.0 | <3.0 | <3.0 | <3.0 | <3.0 |
| D50(μm) | <1.0-5.0 | <1.0 | <1.0-1.5 | <1.0-1.5 | <120 |
| Yankin saman (m2/g) | 8-15 | 6-12 | 6-15 | 8-15 | 0-30 |
| Nau'in Kayayyakin | Nau'in samfur | |||
| Haɗin Sinadari | CeriumdaidaitaZrO2 | Magnesium ya daidaitaZrO2 | Calcium ya daidaita ZrO2 | Zircon aluminum hada foda |
| ZrO2+HfO2 % | 87.0 ± 1.0 | 94.8 ± 1.0 | 84.5 ± 0.5 | ≥14.2±0.5 |
| CaO | --- | --- | 10.0± 0.5 | --- |
| MgO | --- | 5.0± 1.0 | --- | --- |
| CeO2 | 13.0 ± 1.0 | --- | --- | --- |
| Y2O3 % | --- | --- | --- | 0.8 ± 0.1 |
| Al2O3 % | <0.01 | <0.01 | <0.01 | 85.0 ± 1.0 |
| Fe2O3% | <0.002 | <0.002 | <0.002 | <0.005 |
| SiO2 % | <0.015 | <0.015 | <0.015 | <0.02 |
| TiO2% | <0.005 | <0.005 | <0.005 | <0.005 |
| Haɗin Ruwa (wt%) | <1.0 | <1.0 | <1.0 | <1.5 |
| LOI(wt%) | <3.0 | <3.0 | <3.0 | <3.0 |
| D50(μm) | <1.0 | <1.0 | <1.0 | <1.5 |
| Yankin saman (m2/g) | 3-30 | 6-10 | 6-10 | 5-15 |
Samar da duwatsu masu daraja na zirconia daga zirconia foda wani muhimmin filin aiki ne mai zurfi na zirconia da aikace-aikace. The roba cubic zirconia mai wuya ne, marar launi, kuma crystal mara lahani. Saboda ƙarancin tsadarsa, mai dorewa, da kamanninsa ga lu'u-lu'u, gemstones na cubic zirconia gemstones sun kasance mafi mahimmancin madadin lu'u-lu'u tun 1976.
Idan kuna da wasu tambayoyi. Don Allah jin daɗin tuntuɓar mu.