Foda alumina don gogewa
Ƙara Koyo- Launi:Fari
- Siffa:Foda
- Kayan aiki:Al2O3
- Siffar lu'ulu'u:Tsarin Kiristal Mai Tauri
- Yawan gaske:3.90 g/cm3
- Wurin narkewa:2250 °C
- Matsakaicin zafin aiki:1900 °C
- Taurin Mohs:9.0-9.5
- Micro taurin:2000 - 2200 kg/mm2
-
Kayan aikin gogewa na niƙa 240#-12500# Foda mai farin Alumina
Ƙara Koyo- Launi:Tsarkakken Fari
- Siffa:Mai siffar cubic da kusurwa da kaifi
- Takamaiman Nauyi:≥ 3.95
- Taurin Mohs:9.2 Mohs
- Wurin narkewa:2150℃
- Yawan yawa:1.50-1.95g/cm3
- Al2O3:Minti 99.4%
- Na2O:0.30%Matsakaicin
-
Masana'antar samar da foda na Alumina Oxide don Shafi
Ƙara Koyo- Matsayin Samfuri:Foda Fari
- Bayani dalla-dalla:0.7 um-2.0 um
- Tauri:2100kg/mm2
- Nauyin kwayoyin halitta:102
- Wurin Narkewa:2010℃-2050℃
- Wurin Tafasawa:2980℃
- Ruwa Mai narkewa:Ba ya narkewa a cikin ruwa
- Yawan yawa:3.0-3.2g/cm3
- Abubuwan da ke ciki:99.7%
-
Mai ƙera Farin Aluminum Oxide mai Tsarkakakken Tsarkaka
Ƙara Koyo- AlO3:99.5%
- TiO2:0.0995%
- SiO2 (ba kyauta ba):0.05%
- Fe2:0.08%
- MgO:0.02%
- Alkali (Soda da Potash):0.30%
- Siffar Lu'ulu'u:Ajin Rhombohedral
- Yanayin Sinadarai:Ampphoteric
- Takamaiman Nauyi:3.95 grm/cc
- Yawan Yawa:116 lbs/ ƙafa 3
- Tauri:KNOPPS = 2000, MOHS = 9
- Wurin Narkewa:2,000°C
-
Farin Fused AluminA Nika Mai Tsabtace Sandblasting Babban Matsayi Mai Tsabtace
Ƙara Koyo- AlO3:99.5%
- TiO2:0.0995%
- SiO2 (ba kyauta ba):0.05%
- Fe2:0.08%
- MgO:0.02%
- Alkali (Soda da Potash):0.30%
- Siffar Lu'ulu'u:Ajin Rhombohedral
- Yanayin Sinadarai:Ampphoteric
- Takamaiman Nauyi:3.95 grm/cc
- Yawan Yawa:116 lbs/ ƙafa 3
- Tauri:KNOPPS = 2000, MOHS = 9
- Wurin Narkewa:2,000°C
-
F12-F220 Farin Alumina Oxide Grits
Ƙara Koyo- Al2O3:99.5%
- TiO2:0.0995%
- SiO2:0.05%
- Fe2:0.08%
- MgO:0.02%
- Takamaiman Nauyi:3.95 grm/cc
- Tauri:Mohs 9
- Wurin Narkewa:2,000°C